DAKAI

Grades

Grades and properties

Six grades we roll every week, with the data engineers ask for first.

All grades: OD 6–630 mm, WT 0.5–50 mm, length 5800–6000 mm or random, ends plain or beveled, surface pickled / annealed / bright annealed. New mill material with MTC to EN 10204 3.1.

Austenitic stainless · general purpose

TP304 / 304L

The most widely used austenitic grade. Good corrosion resistance, excellent formability and weldability; general piping, food equipment, architecture and decor.

Standards
ASTM A312 / ASME SA312 / GB/T 14976 / EN 10216

Low-carbon austenitic · corrosion resistant

TP316L

Molybdenum-bearing low-carbon stainless with superior pitting and chloride resistance; chemical processing, marine, heat exchangers and pharmaceutical equipment.

Standards
ASTM A312 / ASME SA312 / GB/T 14976 / EN 10216

Ti-stabilised austenitic · high temperature

TP321

Titanium-stabilised grade with excellent intergranular corrosion resistance after welding; service up to 870 °C, boiler tube, exhaust and furnace components.

Standards
ASTM A312 / ASME SA312 / GB/T 14976

Heat-resisting austenitic · high temperature

310S

High chromium-nickel grade for continuous service up to 1100 °C, with excellent oxidation and carburisation resistance; furnace rolls, burners and heat-treatment equipment.

Standards
ASTM A312 / ASME SA312 / GB/T 14976

Duplex stainless · high strength

2205 (S31803 / S32205)

Ferrite-austenite duplex with roughly double the yield strength of austenitic grades, excellent SCC and pitting resistance; oil and gas, desalination, chemical and marine.

Standards
ASTM A790 / ASME SA790 / UNS S32205

Super duplex · severe corrosion

2507 (S32750)

25% Cr, 7% Ni and 3.5% Mo with PREN above 40; exceptional pitting, crevice and SCC resistance in chloride service; offshore, seawater and chemical processing.

Standards
ASTM A790 / ASME SA790 / UNS S32750

Composition and mechanical properties

Reference values for grade selection; the MTC for each batch is the binding document.

Chemical composition (wt%)

GradeCCrNiMoNOthers
TP304 / 304L0.08 / 0.03518.0–20.08.0–12.0——Mn ≤ 2.0, Si ≤ 1.0
TP316L0.03516.0–18.510.0–14.02.0–3.0—Low carbon, pitting resistant
TP3210.0817.0–19.09.0–12.0——Ti ≥ 5 × C (0.40–0.70)
310S0.0824.0–26.019.0–22.0——Heat resisting, to 1100 °C
22050.03022.0–23.04.5–6.53.0–3.50.14–0.20Duplex, high strength
25070.03024.0–26.06.0–8.03.0–5.00.24–0.32Super duplex, PREN 40+

Mechanical properties (annealed, minimum typical)

GradeTensile (MPa)Yield 0.2% (MPa)Elongation (%)Hardness (HB max)
TP304 / 304L515 (75 ksi)205 (30 ksi)40187
TP316L485 (70 ksi)170 (25 ksi)40187
TP321 / 310S515 (75 ksi)205 (30 ksi)35187
2205620 (90 ksi)450 (65 ksi)25290
2507750 (109 ksi)550 (80 ksi)15290

Values are typical per ASTM A312 / A790 and EN 10216. Ask us for a specific heat or a tighter range.

Send your size list or drawing. Get a quotation within 24 hours.